SIFAT MEKANIK POLIMER KOMPOSIT SERBUK BONGGOL JAGUNG DENGAN VARIASI KOMPOSISI RESIN DAN KATALIS

Pratomo, Wahyu (2019) SIFAT MEKANIK POLIMER KOMPOSIT SERBUK BONGGOL JAGUNG DENGAN VARIASI KOMPOSISI RESIN DAN KATALIS. Undergraduate thesis, Politeknik Negeri Jember.

[img] Text (Abstract)
07. ABSTRACT.pdf - Submitted Version
Available under License Creative Commons Attribution Share Alike.

Download (90kB)
[img] Text (Bab 1 Pendahuluan)
15. BAB 1. PENDAHULUAN.pdf - Submitted Version
Available under License Creative Commons Attribution Share Alike.

Download (82kB)
[img] Text (Daftar Pustaka)
20. DAFTAR PUSTAKA.pdf - Submitted Version
Available under License Creative Commons Attribution Share Alike.

Download (80kB)
[img] Text (Laporan Lengkap)
22. B43140566_LAPORAN LENGKAP.pdf
Restricted to Registered users only

Download (1MB)

Abstract

This research was conducted to determine the results of tensile strength and impact toughness of corncob powder. Corn weed is a waste which is very minimal, people use it. In making composite specimens consists of 2 matrix compilers and reinforcemen. The making of specimens was carried out using variations in the form of (%) resin compositions and corncob powder, where the composition included 39.2: 60.8, 49.1: 50.9 and 49.4: 50.5 volume and weight reactions, followed by tensile testing and impact testing. the impact test of the largest value in the comparison to 3 is (49.4: 50,5) the results are 0.2634 J / mm2, and the smallest results are in the ratio of 2 (50:50) which is 0.1934 J / mm2. these results show that if the fibers that hold a lot more than the resin can hold more strokes that occur against the specimen, while the toughness values obtained are the highest at the ratio (39.2: 60.8) of 15, 93367 J / mm2, and the lowest result lies in the 2nd ratio (49.1: 50,9) which is 12.75467 J / mm2. In the tensile test the maximum ratio of comparison to 1 (39.3: 60,6) is: 97,724 (N / mm2), for comparison to 2 (49,1: 50,8) of: 98,431 (N / mm2), and for comparison to 3 (50.3: 49,6), namely: 45,425 (N / mm2), while the strain is generally a comparison to 1 (39,3: 60,6), namely: 0,256 (mm / mm), in comparison to 2 (49,1: 50,8) reached: 0,307 (mm / mm), and in comparison to 3 (50,3: 49,6) of: 0,369 (mm / mm) Keywords: Corn Bump, Weight Fraction (%), Strain stress

Item Type: Thesis (Undergraduate)
Contributors:
ContributionContributorsNIDN/NIDK
Thesis advisorTvagita, Dicky AdiNIP19890622201831001
Subjects: 410 - Rumpun Ilmu Teknik > 430 - Ilmu Keteknikan Industri > 431 - Teknik Mesin (dan Ilmu Permesinan Lain)
Divisions: Jurusan Teknik > Prodi D4 Mesin Otomotif > Tugas Akhir
Depositing User: Sri Supriyatiningsih
Date Deposited: 08 Jan 2026 01:16
Last Modified: 08 Jan 2026 01:16
URI: https://sipora.polije.ac.id/id/eprint/50114

Actions (login required)

View Item View Item